Condensation type rubber pad printing
Product Name:
Condensation type rubber pad printingModel No.:
普配Price:
时价Minimum Order:
20
Product Abstract:
Condensation type rubber pad printing is used for surface printing, such as plastic hardware products have excellent durable grinding performance, no deformation, no oil and the good properties, such as printing ink transfer.- Product Description
A, properties and USES
1, rubber pad printing is a two-component RTV silicone rubber, can be at room temperature vulcanization molding, curing time varies with the amount of curing agent, the more the amount of curing agent, curing the faster.
2, condensation type rubber pad printing is used for surface printing, such as plastic hardware products have excellent durable grinding performance, no deformation, no oil and the good properties, such as printing ink transfer.
Second, the typical physical properties
Physical properties
unit
528 #
755 #
609 #
608 #
606 #
2116 #
766 #
7525 #
color
\
white
white
yellow
white
white
white
white
yellow
viscosity
MPa. S
32000
32000
38000
22000
28000
28000
38000
380000
Curing agent
\
30 # T -
30 # T -
30 # T -
30 # T -
30 # T -
30 # T -
30 # T -
CAT 40 # -
Mixing ratio
\
2%
2%
2%
2%
2%
2%
2%
2.5%
Operating time
Mins
8-15
8-15
8-15
8-15
8-15
8-15
8-15
10-20
Cure time
To pump
2-4
3-5
2-4
3-5
2-4
2-4
2-4
2-4
hardness
Shao A (24 h)
25 + 2
24 + 2
25 + 2
24 + 2
25 + 2
25 + 2
25 + 2
29 + 2
The tensile strength
Mpa (24 h)
2.2
3
3
1.5
3.3
3.5
3.0
3.0
Tear strength
KN/m (24 h)
8.0
16
5
3
6
18
16
5.3
Physical properties
unit
2121 #
233 #
282 #
686 #
811 #
729 #
688 #
535 #
color
\
yellow
red
red
red
red
red
red
white
viscosity
MPa. S
38000
32000
30000
28000
28000
28000
28000
32000
Curing agent
\
30 # T -
8 # M -
30 # T -
30 # T -
30 # T -
7 #
30 # T -
The CAT - 40
Mixing ratio
\
2%
2.5%
2%
2%
2%
2%
2%
2.5%
Operating time
Mins
8-15
10-20
8-15
8-15
8-15
8-15
8-15
10-20
Cure time
To pump
2-4
2-4
2-4
3-5
2-4
2-4
2-4
2-4
hardness
Shao A (24 h)
25 + 2
31 + 2
27 + 2
25 + 2
25 + 2
23 + 2
25 + 2
30 + 2
The tensile strength
Mpa (24 h)
3.5
2
2.8
3.5
3.0
3.5
3.5
3.3
Tear strength
KN/m (24 h)
18
5.5
17
5.5
18
18
18
10
Third, use process
1. According to the proportion of each component in the formula, to calculate the first to operate rubber head size, and then work out the weight of each group, and in a fixed container.
2. Stir the mixture in the mixer fully, mixing, form a stable, consistent color liquid.
3. The mixed liquid in vacuum processing in the vacuum vessel.
4. Good vacuum rubber mixture has clean the blister mould or crystal mould of sulfide.
Four, packaging, storage and transportation and matters needing attention:
1. This series product base gum with 200 kg, 25 kg, 5 kg and 1 kg packing.
2. The series of products should be sealed storage, and in a cool place, prevent the rain, the sun exposure.
3. This series product is a non-dangerous goods, but should pay attention to in use process, avoid the curing agent contact with skin and eyes. With the right amount of detergent and water, immediately if cleaning, such as the eyes, with flowing water washing at least 15 minutes, and consult a physician.
- Related Products
- [Return Home] [Print] [Go Back]
Products Search
Brand Zone
Contact Us
Contact Person:
Xiaohai QiTel:
+8613533634945Fax:
Renewable resources, reasonablyE-mail:
158354113@qq.com-